Thermal Conductivity
11.7Wm-k
Working Temperature
-30~280 degree celsius
Density @ 20℃ (g/ml)
3.25
Viscosity @ 1rpm (m.Pa s)
80,000
Thermal Impedance
0.0016℃-in²/W
Permittivity @ 106Hz
2
Volume Resistivity
3.0x10x(Ohm.cm)
Dielectric Strength
2.0KV/mm